Nature
Emulgent
colloid
protector
system
Solids
content
(%)
Brookfield viscosity
RVT 20ºC
20 rpm (cps)
pH
Minimum skin
forming time
Specific weight
20ºC
(gr/cm3)
ADICRIL VHDP-42
vinyl
alcohol polyvinyl
40
8000-14000
4-5
0ºC
1,02
ADICRIL VCD-57
vinyl–acrylic
cellulose derivative
56
3500-6500
4,5-5,5
10ºC
1,07
ADICRIL VCD-240
vinyl-veova
cellulose derivative
55
4000-8000
4,5-5,5
15ºC
1,07
ADICRIL VCD-245
vinyl-veova
cellulose derivative
55
3000-7000
4,5-5,5
18ºC
1,07
ADICRIL ASD-90
acry.-styrene
surf. ten.reducer
50
1200-5000
7-8
20ºC
1,07
ADICRIL ASD-94
acry.-styrene
surf. ten.reducer
50
800-4000
7-8
21ºC
1,07
ADICRIL ASD-96
acry.-styrene
surf. ten.reducer
50
3000-6000
7,5-8,5
0ºC
1,07
ADICRIL ASD-97
acry.-styrene
surf. ten.reducer
50
3000-6000
7,5-8,5
0ºC
1,07
ADICRIL ASD-98
acry.-styrene
surf. ten.reducer
50
1500-5000
7,5-8,5
0ºC
1,07
ADICRIL ARD-750
acrylic
surf. ten.reducer
47
<500
7,5-8,5
10ºC
1,07
ADICRIL ARD-775
acry.-styrene
surf. ten.reducer
41
<500
7-8
28ºC
1,05
ADICRIL ARD-780
acrylic
surf. ten.reducer
44
<500
7,5-8,5
28ºC
1,05
ADICRIL A-47
acrylic
surf. ten.reducer
40
<200
8-8,7
47ºC
1,04
ADICRIL A-50
acrylic
surf. ten.reducer
47
200-800
8-9
6ºC
1,04